I enjoy making fused items, too. I made two plates for Their Majesties lunch at Fall Crown last weekend. I had an issue with the first one, and turned to the great people at Fused Glass Fanatics on Facebook.

The "not quite right" but serviceable plate, in the mold.

I was informed this is called "dog boning" and is the result of firing either too quickly or to too hot a temperature. After giving my firing schedule I was told the pre-set schedule I've been using goes about 100°, maybe 150°, too hot. I'm very glad to know this, and to know there is a term for it!